Predispersed rubber chemical Masterbatch rubber-chemical-masterbatch
Current position : Homepage > Predispersed rubber chemical Masterbatch > Accelerator TMTD-75 Masterbatch

Featured products

Competitive price

  • Rubber accelerator MTT
    Rubber accelerator MTT 2018/03/10

    Konson® Rubber Accelerator MTTChemical Name  :3-Methylthiazolidine-2-Thione Molecular Formula  C4H7NS2...

  • Rubber accelerator TBBS
    Rubber accelerator TBBS 2012/03/15

    Konson® Rubber Accelerator TBBS Chemical Name  N-tert-butyl-2-benzothiazole Sulfenamide Molecular Formula   C11H14N2S...

  • Rubber accelerator MBTS
    Rubber accelerator MBTS 2012/03/13

    Konson® Rubber Accelerator MBTS Chemical Name    2, 2-Dibenzothiazole Disulfide (MBTS)  ...

  • Rubber Accelerator TMTD
    Rubber Accelerator TMTD 2012/03/11

    Konson® Rubber Accelerator TMTD Chemical Name Tetramethyl Thiuram Disulfide Molecular Formula  C6...

Accelerator TMTD-75 Masterbatch

Pubdate:2019/05/06 Predispersed rubber chemical Masterbatch views:323

Konson® Accelerator TMTD-75

Product description

Composition 75% tetramethylthiuram disulphide, 25% EPDM/EVA binder and dispersing agents

Appearance White or light-yellow granules

Density 20 oC Approx. ~ 1.26 g / cm3  (20 oC )

Physiological properties : See safety data sheet (MSDS)

Raw material characteristics of TMTD:

Melting point ~ 140 oC

Evaporation loss ≤ 0.3%

TMTD content ≥ 98%

Sieve residue 63µm ≤ 0.5 %

Ash content ≤ 0.3 %

Use Characteristics A super accelerator Konson® TMTD-75 used as secondary accelerator for NR, SBR, NBR, IIR, BR, and CR. When used together with delayed action accelerators such as CBS and others, Konson® TMTD-75 acts as an activator. It is an activator for basic accelerator, e.g. aldehyde amine and guanidine, and suitable for low temperature curing products. As a sulfurless cuirng agent, It gives good heat resistance and aging resistance. If mercapto or sulphenamide accelerators are added, the vulcanization undergoes retardation. In such cases they have little effect on the degree of crosslinking; they mainly reduce the scorch rate and increase total curing time.

Processing Advantages The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective TMTD is assured.

Dosage levels primary: 0.1 – 1 phr + 3 – 1 phr sulfur;

secondary: 2.75 – 1.75 phr sulfur  and  0.05 – 0.25 phr + 1 – 1.5 phr MBTS;

sulfurless (for heat resistant mixes): 2.5 – 4 phr + 0.5 phr mercaptobenzothiazole.

Applications Heat resistant mechanical articles, cable coverings and insulations.

Packing Net 25 kg cartons with plastic inner.

Storage stability In original closed containers under cool and dry conditions max. 1 years.